Search
.Management Sciences
Category: Dental Materials
Insufficient closure of the flasks during packing of denture base resin can result in_____________?
A. Poor colour stability
B. Less polymerization shrinkage
C. Increase in vertical dimension
D. Decrease in vertical dimension
Residual monomer content of chemically activated resins is______________?
A. 0.2% to 0.5%
B. 2% to 5%
C. 0.3% to 0.5%
D. 2% to 5%
Dentin conditioner has the following function______________?
A. Removes smear layer
B. Increases surface energy of dentin
C. Forms a thin resin layer over exposed collagen fibrils
D. Helps in bonding with composite
One of the most important advantages of truly elastic impression material would be its capacity for______________?
A. Close adaptation to soft tissues
B. With drawl without permanent distortion
C. Reproduction of surface details
D. Compatibility with gypsum products
Cross linking in denture base resin is contributed by_____________?
A. Glycol dimetharylate
B. Benzoyl peroxide
C. N-para toluidine
D. Methyl methacrylate
Plaster mix____________?
A. Rapid spatulation results in decreased setting time
B. 2% potassium sulphate is accelerator
C. Citrates are retarders
D. All of the above
Porosity present in a acrylic denture is usually the result of______________?
A. A prolonged curing cycle
B. Lack of sufficient pressure applied to flask
C. Insufficient acrylic resin monomer
D. Prolonged bench cooling after curing
The rate of tarnish and corrosion of class II cast material having VHN 200 is_______________?
A. 0%
B. 2 to 3%
C. 5 to 10%
D. <1%
According of ADA specification No or number 1, the minimum compressive strength for silver amalgam filling aftr one hour should be________________?
A. 80 Mpa
B. 140 Mpa
C. 260 Mpa
D. 510 Mpa
Recent Comments